| 1.By enlarging the outer fin area yet 22% lighter than factory stock’s, cooling efficiency was increased by 15 to 20 percent. | |
| 2.By using thinner core tube, the weight was reduced by 22 percent maximum. | |
| 3.By increasing the flow cross section of inner tube, pressure loss was decreased by 15 to 20 percent. | |
| 4.Highly durable, heat resistant blue silicone hoses are used for joint hoses. | |
| 5.Piping are designed with minimum bend for minimum flow loss, and Aluminum is used for weight reduction. | |
| 6.Side tanks and piping are polished for “Type R”. It enhances the cool racing look of LM INTECOOLER. | |
|
|